Potter Wheel as Flat Lap

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Indigo S
Posts: 10
Joined: Wed Nov 05, 2014 2:33 pm

Potter Wheel as Flat Lap

Post by Indigo S »

Hi,
Trying to save money- and time here. Wondering if anyone has used a pottery wheel with grit as a flat lap? I can get a used pottery wheel off CL for far less than a flat lap. I know there is a rpm difference with pottery wheels maxing out at 250 rpm. If anyone has ever tried this- or has ideas about it, please let us know. thanks
Rick Wilton
Posts: 273
Joined: Sat Oct 25, 2003 8:18 pm
Location: Calgary, Canada
Contact:

Re: Potter Wheel as Flat Lap

Post by Rick Wilton »

Rick Wilton
charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Potter Wheel as Flat Lap

Post by charlie »

depending upon diameter, you may not want to run a grit lap faster than that anyway. i calculated mine out to around 200 rpm for a 24" disk when i built it.
Soozin
Posts: 11
Joined: Mon Sep 26, 2005 10:40 pm
Location: NEW ZEALAND

Re: Potter Wheel as Flat Lap

Post by Soozin »

Pottery wheels using slurry is fantastic. I have used my old pottery wheels for years for flat lapping but only for 100 grit silicon carbide. When I want to flatten a bottom of a piece, it's a kick wheel, not electric and it's faster than doing it on a piece of glass by hand. The pottery wheel I have is quite small but it has served me well.. I can grind down a say, vessel bottom in less than ten minutes using 100 grit silicone carbide. However, you want to go to a finer grit, ensure you clean off any coarser grit beforehand making sure there's no residue of that coarse grit left, before putting on finer grits... A good hose flush does a good job! I recommend it, my pottery wheel has served me well over the past ten years! It doesn't need power to run it, just the power of the kick wheel bit... so you also get a wee workout...
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Potter Wheel as Flat Lap

Post by Buttercup »

A few years ago we had an excellent thread going with tips for DIY equipment designs and construction but I can't find it now. I searched under my posts, as I know I posted in it, may have even started it, but it doesn't show up. Perhaps it disappeared when the board went down? Does anyone have a link to it? I think it may have been called DIY flat lap or WBS. I'd like to see it again as some good ideas were posted. Jen
peter cummings
Posts: 71
Joined: Mon Jan 19, 2004 4:05 am
Location: sale,s.e.vic,australia
Contact:

Re: Potter Wheel as Flat Lap

Post by peter cummings »

I bought an old potters wheel, electric, and got a steel plate to fit. Magnetic diamond discs from His, 30 cm I think. Fantastic. Sure the discs could go faster, but I feel I have more control at a slower speed. Only part I miss of an old iron disc and grit is the magic singing sound.