glue

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
AJK25
Posts: 41
Joined: Wed Jul 20, 2005 12:49 pm

glue

Post by AJK25 »

Curious if anybody knows of a glue that adheres glass to metal that they think is terrific. I've been using a few glues that are pretty good, but looking for one that is unbelievably good.

Thanks,
Drew Kates
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: glue

Post by Brad Walker »

Silicone
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: glue

Post by Barry Kaiser »

E6000 used correctly, see my tutorial.

Barry
Tom Fuhrman
Posts: 187
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: glue

Post by Tom Fuhrman »

Tangent Industries --VBB
Dick
Posts: 89
Joined: Sun May 01, 2005 9:34 pm
Location: San Diego
Contact:

Re: glue

Post by Dick »

I find that you can not beat Loctite products. their catalog even lists all materials and shows you what glue for what . I use Loctite hysol h30cl. It works great, dries crystal clear and holds a lot of weight.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: glue

Post by Bert Weiss »

Hang your glass is a board sponsor. Click on their link.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
brottworks
Posts: 6
Joined: Mon May 31, 2004 11:34 am
Location: New Orleans
Contact:

Re: glue

Post by brottworks »

I see all responses as great thus far, yet form follows function for me, so never rely on chemical bonds- unless it's absolutely necessary i.e. lamination for IBC + below 18". so I drill holes, run cables, and often sweat solder into copper and brass.
That said I have experimented with all listed and many others- and would choose based the variables of expansion/contraction/moisture intrusion- and most importantly UV stability i.e. will sunlight ever hit this bond.
If yes- use 100% silicone, and with what ever you choose add undercuts to both surfaces as to also make the bond physical. and not just witchcraft...
+ I also love Hextall, https://www.youtube.com/watch?v=i6Ysd04b05Y
for glass to glass, but as I don't know what your gluing, I can't say that's a good choice...
sorry for the ramble...
Best from NOLA
Andy Brott
www.brottworks.com
Post Reply