Doilies and fossil vitrae

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Chester
Posts: 1
Joined: Wed May 06, 2015 8:49 pm

Doilies and fossil vitrae

Post by Chester »

I was wondering if I could use a doily like a fern for fossil vitrae. Would the doily burn cleanly out? Thanks, in advance, for any help you can give me.
Vonon
Posts: 196
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Doilies and fossil vitrae

Post by Vonon »

It seems to me that if ferns and cedar branches work a paper doilie should be OK. There may be a bit of ash left behind but the imprint of the powder or enamel should not be affected.
Vonon
Peter Angel
Posts: 186
Joined: Fri Oct 31, 2008 9:26 am
Location: Newtown, Sydney, Australia.

Re: Doilies and fossil vitrae

Post by Peter Angel »

Hi Chester. Did you end up making the doily fossil? Pete
Peter Angel
http://peterangelart.blogspot.com/