Hi,
I picked up a 16" octagonal ceramic kiln with the standard kanthal side elements. I would like to turn it into a more suitable "glass" kiln by adding an element to the top. I was going to use a router to excavate a deep groove and pin in a Kanthal element. Is there a better way?
Thank you

Bob
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Adding heating element to kiln lid

Post by Brad Walker »

The router will work. Better is quartz tubes with the elements inside (avoids brick dust) or even porcelain rods with elements surrounding.