Hi. I recently bought a flat lap wheel and while I LOVE it, I'm a bit frustrated how to get the dried bits of cerium oxide out of some of the small bubbles after the polishing step. Is it just a matter of wetting the piece and then digging them out with a toothpick?
Any hints or tips would be greatly appreciated.
Thank you, warm glass community!
-Andy
Getting cerium oxide out of small bubbles.
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Getting cerium oxide out of small bubbles.
car wash water jet
Re: Getting cerium oxide out of small bubbles.
Love the soap idea. WIll definitely try it.
Thanks so much.
Thanks so much.
Andy Gersh
andy@andygersh.com
andy@andygersh.com
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Getting cerium oxide out of small bubbles.
The pressure washer at the carwash is the least expensive tool rental out there. You put a few quarters in the machine, and you have a pressure washer in your hand. Bring some foam, to cushion your glass, and shoot away. They even give you the soap.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact:
Re: Getting cerium oxide out of small bubbles.
Buy an old Water Pik at a thrift store. Mini water jet!