Irid

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Joe Wokovich
Posts: 32
Joined: Tue Sep 25, 2007 1:57 pm
Location: Florissant, MO (@ St. Louis, MO)

Irid

Post by Joe Wokovich »

I have an unusual shaped piece of black 96. It would be really great if it was in irid.
I’ve reading around for an answer for what I want to do, but have found nothing.
Is there a glass paint that would simulate the irid coating?
“If you tell me, I will forget.
If you show me, I will remember.
If you let me do it, I will understand."

And then tomorrow I can start all over again
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Irid

Post by Valerie Adams »

AAE Glass is selling a product called Glass Glo paints. They appear to be a dry mica cake that you can wet with water or other mediums. There's a video right now showing that they product an irid-like coating. The nice thing is, they're mixable.

https://www.aaeglass.com/catalogsearch/ ... =glass+glo
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Irid

Post by Bert Weiss »

Joe

Mother of pearl lustre is a good way to add an iridescent coating. The chemicals used on hot glass during manufacture are deadly toxic. The chemicals used in the lustre are not. Choose ceramic or glass based on what temperature you want to work at. You probably want ceramic. The glass ones are designed to apply to drinking glasses and not slump them in the firing. Compatibility is not an issue, because the deposit of chemicals is so thin.

http://www.standardceramic.com/lustres.html
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
glass_affair
Posts: 1
Joined: Mon Oct 12, 2015 4:01 pm

Re: Irid

Post by glass_affair »

Bert Weiss wrote:Joe

Mother of pearl lustre is a good way to add an iridescent coating. The chemicals used on hot glass during manufacture are deadly toxic. The chemicals used in the lustre are not. Choose ceramic or glass based on what temperature you want to work at. You probably want ceramic. The glass ones are designed to apply to drinking glasses and not slump them in the firing. Compatibility is not an issue, because the deposit of chemicals is so thin.

http://www.standardceramic.com/lustres.html

Is there a link to pictures of this type of work? And to instructions on how to use these lustres? Thx
Brad Walker
Site Admin
Posts: 1539
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Irid

Post by Brad Walker »

glass_affair wrote:Is there a link to pictures of this type of work? And to instructions on how to use these lustres? Thx
This is a how-to for pottery, but pretty much the same for glass. https://www.baileypottery.com/glazes/du ... .htm#Pearl Cone 020 is around 1180F, slumping temperature.

If you can find the Mother of Pearl Spray (I don't think it's made anymore), you just spray that on and then fire.

The look is like the inside of a clamshell (hench, the mother of pearl name). It's kind of iridized, but not quite like iridized glass.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Irid

Post by Kevin Midgley »

Use a never used before brush and don't use it in more than one bottle, ie don't mix or you will contaminate it.
Post Reply