Getting cerium oxide out of small bubbles.

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Andy G.
Posts: 11
Joined: Mon Jul 24, 2006 2:34 pm
Location: Burbank, California
Contact:

Getting cerium oxide out of small bubbles.

Post by Andy G. »

Hi. I recently bought a flat lap wheel and while I LOVE it, I'm a bit frustrated how to get the dried bits of cerium oxide out of some of the small bubbles after the polishing step. Is it just a matter of wetting the piece and then digging them out with a toothpick?

Any hints or tips would be greatly appreciated.

Thank you, warm glass community!

-Andy
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Getting cerium oxide out of small bubbles.

Post by Brad Walker »

charlie
Posts: 961
Joined: Mon Mar 10, 2003 3:08 pm

Re: Getting cerium oxide out of small bubbles.

Post by charlie »

car wash water jet
Andy G.
Posts: 11
Joined: Mon Jul 24, 2006 2:34 pm
Location: Burbank, California
Contact:

Re: Getting cerium oxide out of small bubbles.

Post by Andy G. »

Love the soap idea. WIll definitely try it.

Thanks so much.
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Getting cerium oxide out of small bubbles.

Post by Bert Weiss »

The pressure washer at the carwash is the least expensive tool rental out there. You put a few quarters in the machine, and you have a pressure washer in your hand. Bring some foam, to cushion your glass, and shoot away. They even give you the soap.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Getting cerium oxide out of small bubbles.

Post by Valerie Adams »

Buy an old Water Pik at a thrift store. Mini water jet!
Post Reply