OK, this is more kiln related.
I tried calling Paragon, but they don't have business hours on Friday.
So, I programed and fired my school's kiln, a Paragon Dragon. I programed a 300 DPH cool down. I got the FTC message because the kiln naturally cools slower than 300 DPH.
OK, so my question.
We got the error message, but the kiln continued to cool down as per the program, or as closely as possible, right?
We fired pottery and glass, and the kiln had already gone through the anneal zone, but... I'm not sure. This is my students' stuff. I just need reassurance here.
Come on guys. Help a fellow artist out.
FTC Error Message on Paragon Kiln
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: FTC Error Message on Paragon Kiln
You're fine, no problem, don't worry about it.Judd wrote:OK, this is more kiln related.
I tried calling Paragon, but they don't have business hours on Friday.
So, I programed and fired my school's kiln, a Paragon Dragon. I programed a 300 DPH cool down. I got the FTC message because the kiln naturally cools slower than 300 DPH.
OK, so my question.
We got the error message, but the kiln continued to cool down as per the program, or as closely as possible, right?
We fired pottery and glass, and the kiln had already gone through the anneal zone, but... I'm not sure. This is my students' stuff. I just need reassurance here.
Come on guys. Help a fellow artist out.
Flaw in the Orton controller on the Paragon kilns.
-
Arnold Howard
- Posts: 47
- Joined: Mon Oct 13, 2003 5:21 pm
- Location: Converse, Texas USA
- Contact:
Re: FTC Error Message on Paragon Kiln
The Dragon cannot cool at a rate of 300 degrees F per hour, because the walls are thick. (An inch of block insulation is mounted behind the 3" firebricks.) The error code indicates that you programmed a cooling rate that is faster than the kiln is capable of reaching. The error code is merely there to let you know that you should program a slower cooling rate next time.
Sincerely,
Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com
Sincerely,
Arnold Howard
Paragon Industries, L.P., Mesquite, Texas USA
ahoward@paragonweb.com / www.paragonweb.com