soap dish slumping

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
buddys46
Posts: 4
Joined: Wed Nov 10, 2010 10:19 pm

soap dish slumping

Post by buddys46 »

I am using a 4x6 piece of fibreboard 1/2 thick. It has a3/4 inch edge around it. So basically a rectangle with the center cut out. I slumped my glass but the bottom is curved causing the dish to rock. I am just placing the board on my kiln shelf. Is the rocking due to the fact my board is not high enough?? Thanks
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: soap dish slumping

Post by The Hobbyist »

Your rounded bottom could be caused a couple ways.

One is that the slump isn't allowed to go long enough to get the glass all the way down. (most likely)

Second: the fiberboard may have some "give" to it allowing the glass to push into it.

You should, instead, use a fiber rectangle with the center cut out of it. That way the glass could slump down to the kiln shelf and flatten. As If it were a drop ring.

A flat lap or belt sander will correct the curved bottom.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Vonon
Posts: 197
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: soap dish slumping

Post by Vonon »

Is the blank you used 2 layers of glass or just one? Sometimes a single layer will not slump completely.
Vonon
Post Reply