Post by Barbl123 »

Looking to do a square drop bowl -looking for a basic (starting) drop schedule - I have an Olympic champ kiln -any suggestions will be welcomed! :wink:
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Drop Bowl Schedule

Post by Brad Walker »

How large is the hole? How deep is the drop?
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Drop Bowl Schedule

Post by Marty »

How thick the glass?
Which glass?
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Drop Bowl Schedule

Post by JestersBaubles »

Given no other information, this should get you started:

https://creativeparadise.biz/glass/tuto ... ng-project