Bullseye 1015

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Michelle Schouten
Posts: 12
Joined: Thu Nov 16, 2006 12:05 pm

Bullseye 1015

Post by Michelle Schouten »

Does anyone out have experience with bullseye 1015 ? I'm wondering what variation may happen with multiple layers of silver between clear and 1015 on top?
Also has anyone experienced the spread of the reaction outside of the 1015 that bullseye warns about in their notes on 1015?