Where can I get/make glass paints for screen printing?

Post by BillsBayou »

I want to do liquid screen printing, not the powder kind. Where can I get glass paints in larger quantities than I find with Glassline paints? I want to buy a pint/500ml of glass paint.

I'll even accept a good recipe for glass paint using a liquid media and pigments.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Where can I get/make glass paints for screen printing?

Post by Kevin Midgley »

thompson enamels
Don Burt
Posts: 580
Joined: Sun Mar 09, 2003 8:45 pm
Location: Bloomington, Indiana
Contact:

Re: Where can I get/make glass paints for screen printing?

Post by Don Burt »

Reusche & Co. of T.W.S., Inc

http://reuscheco.com
Bert Weiss
Posts: 2339
Joined: Tue Mar 11, 2003 12:06 am
Location: Chatham NH
Contact:

Re: Where can I get/make glass paints for screen printing?

Post by Bert Weiss »

Right from Warm Glass Studio's store
http://www.warmglass.org/enamels

You can mix the medium in yourself. It's not hard to do.
Bert

Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Where can I get/make glass paints for screen printing?

Post by Barry Kaiser »

Kaiser Glass Paints....Made for screen printing
Tod
Posts: 36
Joined: Tue Feb 14, 2006 5:47 pm
Location: Massachusetts

Re: Where can I get/make glass paints for screen printing?

Post by Tod »

I mixed Reusche's tracing black (and others - didn't seem to matter) with squeegee oil from Ulano, but I'd guess that there are many suppliers of screening media.