I want to do liquid screen printing, not the powder kind. Where can I get glass paints in larger quantities than I find with Glassline paints? I want to buy a pint/500ml of glass paint.
I'll even accept a good recipe for glass paint using a liquid media and pigments.
Where can I get/make glass paints for screen printing?
Moderators: Brad Walker, Tony Smith
-
BillsBayou
- Posts: 36
- Joined: Wed Oct 29, 2014 1:08 pm
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Where can I get/make glass paints for screen printing?
thompson enamels
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Where can I get/make glass paints for screen printing?
Right from Warm Glass Studio's store
http://www.warmglass.org/enamels
You can mix the medium in yourself. It's not hard to do.
http://www.warmglass.org/enamels
You can mix the medium in yourself. It's not hard to do.
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: Where can I get/make glass paints for screen printing?
Kaiser Glass Paints....Made for screen printing
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
Re: Where can I get/make glass paints for screen printing?
I mixed Reusche's tracing black (and others - didn't seem to matter) with squeegee oil from Ulano, but I'd guess that there are many suppliers of screening media.