Has anyone used UGC Accents with Bullseye?

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
helenM
Posts: 19
Joined: Tue Feb 23, 2016 9:45 am

Has anyone used UGC Accents with Bullseye?

Post by helenM »

I've been thinking about getting some UGC Accents in gold, bronze or platinum as I'd like some of these mettalic colours in my designs. But the supplier I can get them from doesn't state what glass COE they are compatible with (and haven't replied to my enquiry about it). I use Bullseye glass, so was wondering if anyone here has ever used them with BG, and if so do they give a nice mettalic effect or more of a matt effect.
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Has anyone used UGC Accents with Bullseye?

Post by Brad Walker »

They should work with just about any glass that can be fired in the 1500F range. It's a thin enough layer that COE isn't really a significant issue.
helenM
Posts: 19
Joined: Tue Feb 23, 2016 9:45 am

Re: Has anyone used UGC Accents with Bullseye?

Post by helenM »

Thanks very much for your advice Brad. I'm excited to give this a go.
Post Reply