Post by Geo »

The recent events has made me wonder about just what is happening to the air in my own studio if I'm fusing or casting with red colored glass, for instance. Any thoughts?
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Emissions and studio safety

Post by Brad Walker »

Geo wrote:The recent events has made me wonder about just what is happening to the air in my own studio if I'm fusing or casting with red colored glass, for instance. Any thoughts?
The problem occurs when the glass is being made, heated to 2400F or thereabouts, and some of the chemical components go up the smokestack and into the air. So long as you're just fusing or casting, no issue, any potentially hazardous chemicals are not released.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Emissions and studio safety

Post by Marty »

But there's binders in the refractories that burn off, dusts from working with powders and from sandblasting, mists from coldworking. Common sense ventilation takes care of most, particle masks the rest.
Greg Rawls
Posts: 147
Joined: Sun Mar 09, 2003 8:11 pm
Location: Charleston, SC
Contact:

Re: Emissions and studio safety

Post by Greg Rawls »

Greg