bubble up

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
jim simmons
Posts: 478
Joined: Sun Mar 09, 2003 10:37 pm
Location: Hillsboro Oregon
Contact:

bubble up

Post by jim simmons »

What in the devil is this. This is the first time that I have heard this term
Jim
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: bubble up

Post by JestersBaubles »

aka Boiled glass, I think.

Dana W.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: bubble up

Post by Kevin Midgley »

It is a great way to get the COE to shift.
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: bubble up

Post by Judd »

You can achieve boiled glass (or the effect) with lower temps and longer holds. Still, some COE shift occurs.