Vermiculite Board

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Terry Crider
Posts: 10
Joined: Mon Jul 25, 2005 4:17 pm
Location: Western Ohio

Vermiculite Board

Post by Terry Crider »

I am building a small kiln (a cubic ft.) --- I've seen different boards mentioned to line the kiln with.
Delphi Glass has a Vermiculite Board (their number 92807) --- is this something that will work for the inside liner?
The outside will be IFB's.
I have ceramic blanket left over from our hot glass/batch days --- but I thought some kind of board would be easier
to work with on the walls.
Thanks,
Terry
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Vermiculite Board

Post by Marty »

I'd put the IFB on the inside. VB on the hotface will break down eventually and give you crumbles in your glass (although vacuuming before every firing will help with that).
Actually, if you lay the brick on the flat (dry, no mortar) you get a 4" thick wall that won't need anything else, not for liner nor coldface backup, no metal jacket either.
Use fiber board for the lid and suspend the elements in quartz tubing (assuming a top-loader).
Terry Crider
Posts: 10
Joined: Mon Jul 25, 2005 4:17 pm
Location: Western Ohio

Re: Vermiculite Board

Post by Terry Crider »

Is there a Brand name I can google for the lid material ?
Terry
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Vermiculite Board

Post by Marty »

lots of manufacturers- google refractory fiber board, find someone local.