I have a slumped piece that i need flat so that i can add glass to cover a sand blasted name.
I don't think re-fusing will get it perfectly smooth.
It's on 2 sheets 3mm one fuse one slump just concerned about 3 more firings. Its a lot!!
Thoughts and firing schedule would be very much appreciated .
Thanks
Andrea
re-fusing flat
Moderators: Brad Walker, Tony Smith
re-fusing flat

"C'est Moi (Its Me)"
-
Kevin Midgley
- Posts: 773
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: re-fusing flat
1flatten fire it.
2Flip it over so blasting is down and fire it so as to eliminate the blasting.
3Flip it over to refire it to a nice finish.
4Kiln form it..
You might be able to combine 3 and 4 in one firing.
You might be able to eliminate step 2 by adding a layer of clear but you might also have a ghost image of the blasting.
The quickest solution is to remake the piece.
2Flip it over so blasting is down and fire it so as to eliminate the blasting.
3Flip it over to refire it to a nice finish.
4Kiln form it..
You might be able to combine 3 and 4 in one firing.
You might be able to eliminate step 2 by adding a layer of clear but you might also have a ghost image of the blasting.
The quickest solution is to remake the piece.