How to adhere stand up project to a glass base
What is the best method and glue to adhere a stand up glass project to a glass base?
			
			
									
						
										
						- 
				JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: How to adhere stand up project to a glass base
Depends upon the shape of the glass you are gluing to the base. If it has some means of support in its inherent design, you could use something as simple as E6000. I recently wrote a blog post on a candle shield, that might be helpful:
http://jestersbaubles.blogspot.com/2016 ... hield.html
If the glass piece can't support itself very well against gravity I would use something like HXTAL.
 I would use something like HXTAL.
Dana W.
			
			
									
						
										
						http://jestersbaubles.blogspot.com/2016 ... hield.html
If the glass piece can't support itself very well against gravity
 I would use something like HXTAL.
 I would use something like HXTAL.Dana W.
- 