Hi, I've just bought a diamond pad to grind some glass edges before fire polishing (and to learn how to use it - just bought Paul Tarlow's book to help, excellent book) but I was wondering what the best way of disposing the waste glass is. I thought I would do the grinding in water, let it settle then drain of what water I could and throw the rest in a plastic bag and wrap up for throwing away in my normal waste. 
What do other people do when coldworking? I live in the UK so I'm not sure if there are any rules about this (may have to do a bit of research on that). Also I like to be as ecofriendly as possible when disposing of waste craft products.
			
			
									
						
										
						What do other people do when coldworking? I live in the UK so I'm not sure if there are any rules about this (may have to do a bit of research on that). Also I like to be as ecofriendly as possible when disposing of waste craft products.
- 
				jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Disposing of ground glass
I,personally do not consider ground glass as a hazard to anything but plumbing. I treat it as I would diatomaceous earth and spread it around plants in the garden.
			
			
									
						
							"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
			
						- 
				JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
- 
				Ed Cantarella
- Posts: 155
- Joined: Mon Feb 26, 2018 3:49 pm
- Location: Highland, Michigan, USA
Re: Disposing of ground glass
Just run it down the largest drain in the house - probably the toilet.  Seriously - you've probably washed larger grains of sand off vegetables from the store.
			
			
									
						
							HER last words were, "I'm melting, melting . . . "   Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.
			
						Re: Disposing of ground glass
DON'T put it down the toilet if you have a worm-powered sewage system. It'll tear their little guts out!
			
			
									
						
										
						Re: Disposing of ground glass
Don't put it down ANY drain.
			
			
									
						
										
						- 
				Ed Cantarella
- Posts: 155
- Joined: Mon Feb 26, 2018 3:49 pm
- Location: Highland, Michigan, USA
Re: Disposing of ground glass
OP is only talking a little powder - what's the harm? Glass is sand(roughly), sand is glass. We all habitually wash dirty clothing with embedded sand down the drain and same for dirty vegetables,dogs, etc. And we eat a fair amount which comes out . .Marty wrote:Don't put it down ANY drain.
 . https://health.howstuffworks.com/wellne ... t-year.htm
 . https://health.howstuffworks.com/wellne ... t-year.htmBut I would fully agree that one shouldn't dump grinder sludge down a drain - the particles are much too large to be carried away and could start to accumulate in the trap (u-shaped piece on the drain pipe).
HER last words were, "I'm melting, melting . . . "   Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.
			
						- 
				Terry Crider
- Posts: 10
- Joined: Mon Jul 25, 2005 4:17 pm
- Location: Western Ohio
Re: Disposing of ground glass
Any thoughts on washing very small brushes out in the bath room sink --- Brad's and Barry K's "paints"
			
			
									
						
										
						- 
				Barry Kaiser
- Posts: 311
- Joined: Mon Jul 25, 2005 6:54 pm
- Location: North Carolina
- Contact:
Re: Disposing of ground glass
Terry,
The politically sensitive answer is to not do so.
I did it all the time. Our paints contain very little (relatively) solids and those are ultra fine.
However, I have now installed a Gleko Trap since I do a lot (and I mean a lot) of painting and washing. After the first year, I cleaned out the trap and it was amazing how little solids there was.
Barry
			
			
									
						
							The politically sensitive answer is to not do so.
I did it all the time. Our paints contain very little (relatively) solids and those are ultra fine.
However, I have now installed a Gleko Trap since I do a lot (and I mean a lot) of painting and washing. After the first year, I cleaned out the trap and it was amazing how little solids there was.
Barry
Barry Kaiser
http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
			
						http://www.Kaiserglass.com
glass classes;
http://kaiserglass.com/classes.html[b]
Tutorials; [/b]
http://kaiserglass.com/tutorials.html[b]
Facebook:[/b]
http://www.facebook.com/Kaiserglassdesigns
- 
				JestersBaubles
- Posts: 705
- Joined: Fri Feb 25, 2011 12:01 am
- Location: North Logan, UT
- Contact:
Re: Disposing of ground glass
I have a Gleco trap on my utility sink. I wash anything glass related in that sink (glass itself, brushes, etc). If the piece is small enough, I'll coldwork with handpads in that sink. The grinder sludge, I scrape out and dispose of. Other coldworking water usually ends up in the yard (the water bucket for the lap grinder & saw). 
The utility sink is also great for washing dirty vegetables .
 . 
Dana
			
			
									
						
										
						The utility sink is also great for washing dirty vegetables
 .
 . Dana