I've searched but am unable to find any information on using silver foil on the top layer of glass. Is it food safe or should I be sandwiching it in between two sheets. Thanks for any help.
Patty

It often shows a command of language to say nothing - author unkown.
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Silver Foil

Post by jim burchett »

Since Silver is commonly used in eating utensils I would imagine that it is food safe. Dont see why being on glass would change that.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Silver Foil

Post by Kevin Midgley »

If not sandwiched will it not be subject to the atmosphere, tarnish and wear in other ways? :-k
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Silver Foil

Post by Brad Walker »

Kevin Midgley wrote:If not sandwiched will it not be subject to the atmosphere, tarnish and wear in other ways? :-k
Yes, if not sandwiched it will tarnish, lose its silver sheen, and become brownish-black in a few years.

If you want to avoid this, I would cap with clear or cover with a thin layer of clear powder.
grammy
Posts: 26
Joined: Fri Nov 17, 2006 10:07 am
Location: Charlotte NC
Contact:

Re: Silver Foil

Post by grammy »

Where do you get silver foil? I went to Michaels and that did not look like real silver to me. :shock:
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Silver Foil

Post by Buttercup »

Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Silver Foil

Post by Barry Kaiser »

Ebay.
Lots of places out of India
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Silver Foil

Post by JestersBaubles »

The hobby stores typically only sell real copper, everything else is aluminum.

Just about any art glass supplier will have silver foil. Amazon has pure silver foil, too.