How open should the kiln be

Post by Havi »

Hello everybody'

I am firing with glues and staff which has bad fumes which should be ventilated.It was advised to keep the kiln open to let the fumes out.

I am using my paragon kiln 1 7" dia. It has a new lid , I believe it is made of fiber. It seems to have burnt at the edges when I kept the lid open, the edges of the lid are black.... therefore I am worried that by having the kiln lid open like this, I am damaging it. Can I have the lid open only 1/4" ? Is this enough to ventilate the kiln?


I'd be grateful for your remarks.
Many thanks in advance
Havi

And a very happy new year to all of you - - -
May you be written and signed for good healthy life....
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: How open should the kiln be

Post by Brad Walker »

Yes, 1/4" should be enough. The black residue is from contaminants that haven't totally burned off. It will burn off in subsequent firings.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: How open should the kiln be

Post by Havi »

Thanks,Brad
However, I am not worried about the color of the lid, as much as I am worried that the lid is getting ruined by being fired like this.

Can you comment on this, Brad? Will the lid be warped being exposed directly to the heat?



H
Haviva Z
- - - - with a smile :)

"Speed comes from the Devil" - (an Arabic proverb)
Image
http://www.havivaz.com
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: How open should the kiln be

Post by Brad Walker »

I don't believe the lid would be damaged in any way.
Havi
Posts: 619
Joined: Wed Jul 02, 2003 6:01 am
Location: Israel
Contact:

Re: How open should the kiln be

Post by Havi »

Very good.


Thanks


Havi