Brad's drop bowl class

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Indigo S
Posts: 10
Joined: Wed Nov 05, 2014 2:33 pm

Brad's drop bowl class

Post by Indigo S »

Hi,

I took Brad's drop bowl class several years ago. Could anyone, please, let me know the name of the board used for molds? And.... putting this out to the glass universe..... has anyone messed up and let a bowl drop too far? Now my vessel is trapped in the mold. I'm thinking I will have to sacrifice one or the other- unless the board is water proof. Any ideas? Thanks
Brad Walker
Site Admin
Posts: 1539
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Brad's drop bowl class

Post by Brad Walker »

Ceramaguard is the name of the board we used. If that's what you used in your failed drop, you can either break the board (pretty easy) or soak it in water until it softens.
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Brad's drop bowl class

Post by jim burchett »

You may be able to enlarge the opening enough to remove the piece and save the ring...its fairly soft
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie