Pot Melt Bubbles and Pits

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Mark Wright
Posts: 49
Joined: Mon Dec 13, 2010 12:43 pm
Location: Raleigh, NC

Pot Melt Bubbles and Pits

Post by Mark Wright »

Is there any way to prevent or get rid of the dozens of small bubbles and pits on the surface of a pot melt? After sandblasting and a second fusing it looks better but the pits are still there.
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: Pot Melt Bubbles and Pits

Post by The Hobbyist »

I always hold my melts at around 1500 F for about 45 min to an hour.

Jim "The Hobbyist"
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
Mark Wright
Posts: 49
Joined: Mon Dec 13, 2010 12:43 pm
Location: Raleigh, NC

Re: Pot Melt Bubbles and Pits

Post by Mark Wright »

My program:
1- 250/hr to 1000 hold 15
2- 250/hr to 1100 hold 15
3- 450/hr to 1685 hold 90
4- AFAP to 1520 hold 45
5- AFAP to 900 hold 60
6- 100/hr to 750 hold 15
Post Reply