healing a broken piece of glas.

Post by jim simmons »

I would like to know how to eliminate/minimize a break.
I have a piece of BE that broke and I still want to use to make a bowl.
Should the break be put on the top or the bottom of the 2 layer stack for the fusing?
Thanks
The other Jim
The Hobbyist
Posts: 311
Joined: Sun Mar 09, 2003 7:09 pm
Location: Sun City West (NW Phoenix), AZ
Contact:

Re: healing a broken piece of glas.

Post by The Hobbyist »

The bottom.