Hello ! I am used to see the COE as COE 96, 92, 104. But now I see this: (11,5 ± 0,3 ) χ 10-6 How can you calculate what the COE is ? Jan de Jong
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: coefficient of expansion
It's written in scientific notation. In our world, just read it as 115 +/- 3 or 112 - 118 if you like. It's a much more precise way of writing 115.