Hi all!
Is there a a prescription of how much glass would flow from an aperture of a certain size for a given time and temperature?
I'm about to cast 8 to 10kg (17 to 22 pounds) of S96 glass from a flower pot into a mould with a core. Because of the core, I will close the stock hole in the center and cut 2 new apertures - round cornered rectangulars, about 1x2cm each. Any predictions of how much time it will take at 840C/1550F?
My kiln is very big and I [u][b]cannot[/b][/u] open it while firing.
Thanks!
Flower pot melting debit at top temperature
Moderator: Brad Walker
-
lucho/lachezar/
- Posts: 15
- Joined: Tue Aug 03, 2004 12:46 pm
- Location: bulgaria
- Contact:
-
Valerie Adams
- Posts: 587
- Joined: Mon Apr 19, 2004 2:49 pm
- Location: Santa Rosa, California
- Contact: