Cutting Very Thick Glass Slabs

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Cutting Very Thick Glass Slabs

Post by Judd »

I put this in the New-Bee section because I must be doing something wrong.

So, I bought the Harbor Freight 10" tile saw.
Love it.
And I bought the His Glassworks blade. This one to be exact:
10 Inch x .040 Inch Result Medium Diamond Blade

So, I'm sawing slabs of glass, approximately 3" wide by 10" long.

It takes FOREVER!!!
OMG, to saw one slab is like 2 hours.

What am I doing wrong?

Should I use a rougher blade, then sand the glass with diamond grit?
Is here a machine that will feed the glass into the blade ?
Am I using the blade wrong?

What?
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Cutting Very Thick Glass Slabs

Post by Kevin Midgley »

you could tie a pail of sand to the cutting table to pull the glass into the saw.
Murphy's law states if something will go wrong it will...especially if you are not there watching.
Only takes a moment with no water to destroy a blade.....

This may be way quicker:
https://www.aliexpress.com/item/1PC-Hea ... st=ae803_1
Tom Fuhrman
Posts: 187
Joined: Mon Mar 10, 2003 11:44 am
Location: eastern Tennessee
Contact:

Re: Cutting Very Thick Glass Slabs

Post by Tom Fuhrman »

you don't say what the thickness of the slabs are. I used to cut slabs that were 1" thick and 12" square in a few minutes with a MK saw and a 10" blade I don't know what you're doing wrong. lots of water , a good saw, and a good blade should do it. I also used to cut large pieces of optical Schott crystal for sculptures that were 3" thick and they never took anywhere close to 2 hours.
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Cutting Very Thick Glass Slabs

Post by Judd »

If it will upload, this is an example of what I'm doing.
Attachments
FB_IMG_1501614184934.jpg
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Cutting Very Thick Glass Slabs

Post by Judd »

the finished product here.
Attachments
FB_IMG_1501614233977.jpg
DonMcClennen
Posts: 381
Joined: Sun Mar 09, 2003 9:09 pm
Location: Ontario

Re: Cutting Very Thick Glass Slabs

Post by DonMcClennen »

You didn't answer the question.. "How thick"??
"The Glassman"
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Cutting Very Thick Glass Slabs

Post by Judd »

Sorry Don, we miscommunicated. I said in the initial post it was 3"x10" long. The block is 3" thick.
Valerie Adams
Posts: 587
Joined: Mon Apr 19, 2004 2:49 pm
Location: Santa Rosa, California
Contact:

Re: Cutting Very Thick Glass Slabs

Post by Valerie Adams »

That saw does a better job with a blade stabilizer on it.
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Cutting Very Thick Glass Slabs

Post by Judd »

I'll try that too. Thank you.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Cutting Very Thick Glass Slabs

Post by Marty »

The Result blades may need to be dressed before the first use to remove any plating material covering the outer layer of diamond. Run the blade (wet) through a chunk of brick or silicon carbide sharpening stone; just a couple of cuts should do it. Some people have a fetish about dressing the blades, sometimes before every cut. Don't.
I've had Result blades that lasted years when treated respectfully.

I just sawed a pattern bar 2" thick by 6" long by 4" wide in half the long way- one 1" cut on top, flip and cut again- it took about 40 seconds and had me wondering- is your plate 3" thick?
What does the whole thing weigh?
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Cutting Very Thick Glass Slabs

Post by Judd »

When I cut my glass blocks, I'm cutting through at least 3" by 6" to 10" inches in length.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Cutting Very Thick Glass Slabs

Post by Marty »

3" wide, ok. How about thickness? Are you making a pot melt (or whatever) that's 3" thick (by 3" wide by 6-10" long)?
Judd
Posts: 295
Joined: Mon Sep 01, 2003 9:45 am
Location: Arkansas

Re: Cutting Very Thick Glass Slabs

Post by Judd »

3" is the thickness. I am sawing through 3" of glass, 10" or so inches in length.
Yeah, I'd doing pattern bars (see pics above).
Post Reply