Paragon E9S help.

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
MikeF
Posts: 3
Joined: Tue Nov 15, 2005 8:42 pm
Location: Western PA

Paragon E9S help.

Post by MikeF »

I was recently gifted an old but very well cared for Paragon E9S and pyrometer. This particular kiln is strictly "plug and play", there is no means of controlling it other than pulling the plug. I am considering picking up an appropriately rated infinite switch, electric box and heavy duty grounded appliance cord (think high capacity solder iron controller). I am sure someone out there has done something along these lines. Am I missing anything? TIA. Mike
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Paragon E9S help.

Post by Brad Walker »

Assuming the wiring is done correctly, the infinite switch should work well.
Post Reply