Hello people
I have troubles in edge fire polishing
I use murano glass. I make plates in first firing, then i cut in small pieces with dish saw and the edge stay rough
Then i need to firepolish the edge in a new firing
I tried some times but the edges stay opaque? Maybe any help from antidevit on the edge? Maybe something wrong in the schedule?
Any help will be appreciated
thanks in advance
mike
edge fire polishing
Moderators: Brad Walker, Tony Smith
-
mikefromitaly
- Posts: 67
- Joined: Thu Apr 03, 2003 7:47 am
- Location: italy-sicily
- Contact:
edge fire polishing
thanks for sharing !
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: edge fire polishing
Keep cut glass wet.
Never let it dry out.
Clean edge with brush.
Wash well
Hand dry with towel.
Never let it dry out.
Clean edge with brush.
Wash well
Hand dry with towel.
-
Brad Walker
- Site Admin
- Posts: 1544
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: edge fire polishing
Clean edges before refiring. Use 600 grit grinder or 400 or better diamond hand pad on edges. Often the saw leaves rough edges that hold dirt and will not shine up easily.
If you provide your schedule we can give your our thoughts on whether that's also a factor.
If you provide your schedule we can give your our thoughts on whether that's also a factor.
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
-
mikefromitaly
- Posts: 67
- Joined: Thu Apr 03, 2003 7:47 am
- Location: italy-sicily
- Contact:
Re: edge fire polishing
Hello people
Thank you for your replies
My.schedule is
0-550 30 min
550 soak 15min
550-690 asap
690 30 min.
690-750 asap
Stop
I also tried to brush The edges with spray A but nothing
After cutting with saw i also try to use grind with a b dry belt to get less rough but nothing
Any help?
Thank you
Mike
Thank you for your replies
My.schedule is
0-550 30 min
550 soak 15min
550-690 asap
690 30 min.
690-750 asap
Stop
I also tried to brush The edges with spray A but nothing
After cutting with saw i also try to use grind with a b dry belt to get less rough but nothing
Any help?
Thank you
Mike
thanks for sharing !
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly
mike from italy
"secret of success?... passion & experience"
http://www.picturetrail.com/mikefromitaly