Microcrystalline Wax

Use this forum for discussion on kiln casting, pate de verre, and related topics.

Moderator: Brad Walker

Post Reply
Chris Lowry
Posts: 51
Joined: Thu Sep 24, 2015 12:35 pm

Microcrystalline Wax

Post by Chris Lowry »

So where do you get wax for molding? I can't believe how expensive the stuff I find is, $140 for 10 lbs. Thanks for any info
Peter McCarthy
Posts: 19
Joined: Wed Feb 22, 2006 10:48 am
Location: Cambridge, MA

Re: Microcrystalline Wax

Post by Peter McCarthy »

I get mine from Reynolds Advanced Materials - http://www.reynoldsam.com. They have 10 stores; I don't know if one is near you. If not, search for other local sculpture supply stores.
Chris Lowry
Posts: 51
Joined: Thu Sep 24, 2015 12:35 pm

Re: Microcrystalline Wax

Post by Chris Lowry »

That looks like a cool website, I honestly didn't see Microcrystalline Wax on there. There are no local stores as I live on Maui so ordering is my only choice.

I did find this place for good cheap Victory Brown Wax. http://shop.clay-planet.com/victory-bro ... e-wax.aspx

Now I just have to figure out what plaster I want to use.

Thanks again
Greg Vriethoff
Posts: 4
Joined: Sun Jul 01, 2007 8:03 pm
Location: Charlotte, NC

Re: Microcrystalline Wax

Post by Greg Vriethoff »

Hi Chris,

If you haven't already gone with someone else you can also try The Compleat Sculptor. I order most of my stuff from them.

$84 for a 10lb slab of Victory Brown.
Greg Vriethoff
Posts: 4
Joined: Sun Jul 01, 2007 8:03 pm
Location: Charlotte, NC

Re: Microcrystalline Wax

Post by Greg Vriethoff »

Oh, just looked at your source. Looks like you found a better deal. =D>
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Microcrystalline Wax

Post by Kevin Midgley »

Ed Cantarella
Posts: 155
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Microcrystalline Wax

Post by Ed Cantarella »

OP - you want hard micro-crystalline. Don't accidentally buy white/amber - soft and flexible. Hard is sometimes referred to as jewelers wax.
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.