Spectrum from Mexico

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
BobbieMatus
Posts: 50
Joined: Tue Jul 08, 2003 12:21 am

Spectrum from Mexico

Post by BobbieMatus »

Has anyone used spectrum coming from Oceanside (mexico). I'm wondering about quality
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Spectrum from Mexico

Post by Brad Walker »

Haven't used any personally, but we've heard mixed reviews. Some say it's ok, some say it's not as good as the original.