German Glass COE 82

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Joel Pfeiffer
Posts: 1
Joined: Thu Dec 28, 2017 12:34 pm

German Glass COE 82

Post by Joel Pfeiffer »

I used to get some float glass compatible frit from C&R Loo
They don not exist anymore. Does anyone have a clue to a distributor
of: Floatglasverschmelzung Made in Germany
there are some specific colors that I am looking for...

Thank your for any help and suggestions
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: German Glass COE 82

Post by Brad Walker »

Armstrong Glass has compatible float COE 82: https://www.armstrongglass.com/products ... sheetglass

I believe that some of their float products are made in Germany.