Disposing of ground glass

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
helenM
Posts: 19
Joined: Tue Feb 23, 2016 9:45 am

Disposing of ground glass

Post by helenM »

Hi, I've just bought a diamond pad to grind some glass edges before fire polishing (and to learn how to use it - just bought Paul Tarlow's book to help, excellent book) but I was wondering what the best way of disposing the waste glass is. I thought I would do the grinding in water, let it settle then drain of what water I could and throw the rest in a plastic bag and wrap up for throwing away in my normal waste.

What do other people do when coldworking? I live in the UK so I'm not sure if there are any rules about this (may have to do a bit of research on that). Also I like to be as ecofriendly as possible when disposing of waste craft products.
jim burchett
Posts: 255
Joined: Sun Jun 29, 2003 4:24 pm
Location: Lenoir, NC

Re: Disposing of ground glass

Post by jim burchett »

I,personally do not consider ground glass as a hazard to anything but plumbing. I treat it as I would diatomaceous earth and spread it around plants in the garden.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Disposing of ground glass

Post by JestersBaubles »

Ditto. Pour it on the plants.

Dana W.
helenM
Posts: 19
Joined: Tue Feb 23, 2016 9:45 am

Re: Disposing of ground glass

Post by helenM »

Thank you!
Ed Cantarella
Posts: 155
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Disposing of ground glass

Post by Ed Cantarella »

Just run it down the largest drain in the house - probably the toilet. Seriously - you've probably washed larger grains of sand off vegetables from the store.
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Disposing of ground glass

Post by Buttercup »

DON'T put it down the toilet if you have a worm-powered sewage system. It'll tear their little guts out!
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Disposing of ground glass

Post by Marty »

Don't put it down ANY drain.
Ed Cantarella
Posts: 155
Joined: Mon Feb 26, 2018 3:49 pm
Location: Highland, Michigan, USA

Re: Disposing of ground glass

Post by Ed Cantarella »

Marty wrote:Don't put it down ANY drain.
OP is only talking a little powder - what's the harm? Glass is sand(roughly), sand is glass. We all habitually wash dirty clothing with embedded sand down the drain and same for dirty vegetables,dogs, etc. And we eat a fair amount which comes out . . :mrgreen: . https://health.howstuffworks.com/wellne ... t-year.htm

But I would fully agree that one shouldn't dump grinder sludge down a drain - the particles are much too large to be carried away and could start to accumulate in the trap (u-shaped piece on the drain pipe).
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.
Terry Crider
Posts: 10
Joined: Mon Jul 25, 2005 4:17 pm
Location: Western Ohio

Re: Disposing of ground glass

Post by Terry Crider »

Any thoughts on washing very small brushes out in the bath room sink --- Brad's and Barry K's "paints"
Barry Kaiser
Posts: 311
Joined: Mon Jul 25, 2005 6:54 pm
Location: North Carolina
Contact:

Re: Disposing of ground glass

Post by Barry Kaiser »

Terry,
The politically sensitive answer is to not do so.
I did it all the time. Our paints contain very little (relatively) solids and those are ultra fine.
However, I have now installed a Gleko Trap since I do a lot (and I mean a lot) of painting and washing. After the first year, I cleaned out the trap and it was amazing how little solids there was.

Barry
JestersBaubles
Posts: 705
Joined: Fri Feb 25, 2011 12:01 am
Location: North Logan, UT
Contact:

Re: Disposing of ground glass

Post by JestersBaubles »

I have a Gleco trap on my utility sink. I wash anything glass related in that sink (glass itself, brushes, etc). If the piece is small enough, I'll coldwork with handpads in that sink. The grinder sludge, I scrape out and dispose of. Other coldworking water usually ends up in the yard (the water bucket for the lap grinder & saw).

The utility sink is also great for washing dirty vegetables :) .

Dana