Skutt km1227 1phase 240v
Moderators: Brad Walker, Tony Smith
Skutt km1227 1phase 240v
We have four elements burned out at once. They seem to sell replacements in odd ways....One bottom, one intermediate one top and so on, Aren't they all the same length?Except for possibly the bottom element they all appear to be the same....It seems I could purchase two three packs of elements much cheaper than buying an entire set?
-
Brad Walker
- Site Admin
- Posts: 1539
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Skutt km1227 1phase 240v
Although it varies by manufacturer, the elements aren't all the same. Lengths can differ, as can other element characteristics. I'd stick to their recommendations.
You can also get elements from people other than the manufacturer. Sometimes they're cheaper, sometimes they're not, but they usually need to know more details about the element than the manufacturer requires. If you want to go that route, try Duralite and Euclids.
You can also get elements from people other than the manufacturer. Sometimes they're cheaper, sometimes they're not, but they usually need to know more details about the element than the manufacturer requires. If you want to go that route, try Duralite and Euclids.
-
Tony Smith
- Posts: 1037
- Joined: Sun Mar 09, 2003 5:59 pm
- Location: Massachusetts, USA
- Contact:
Re: Skutt km1227 1phase 240v
It seems bizarre that all 4 elements would burn out at the same time... in fact, I would say the likelihood is near zero. How did you determine that the elements were all burned out?
Thanks
Tony
Thanks
Tony
The tightrope between being strange and being creative is too narrow to walk without occasionally landing on both sides..." Scott Berkun
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
Re: Skutt km1227 1phase 240v
I would bet dollars to donuts that you lost a relay.
The other Jim
The other Jim
Re: Skutt km1227 1phase 240v
When I say burned out I mean they are all broken. They were old and this kiln does numerous frequent firings..Tony Smith wrote:It seems bizarre that all 4 elements would burn out at the same time... in fact, I would say the likelihood is near zero. How did you determine that the elements were all burned out?
Thanks
Tony