When a color doesn't strike

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Laura Walter
Posts: 6
Joined: Mon Nov 22, 2004 2:58 pm

When a color doesn't strike

Post by Laura Walter »

Can a color that didn't strike on the 1st time through the kiln (violet striker, #1234, came out a muddy transparent blue depending on the light) go through the kiln again to reach it's intended color or is it now scrap? I didn't hold it for 2 hours at 1225.
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: When a color doesn't strike

Post by Brad Walker »

To help it strike better hold in the 1225 to 1240F range for half an hour one hour. Two hours is probably overkill.
Laura Walter
Posts: 6
Joined: Mon Nov 22, 2004 2:58 pm

Re: When a color doesn't strike

Post by Laura Walter »

Thanks Brad.
Post Reply