Post by heywilli »

Hi, has anyone used Cristalica 100 nuggets for casting yet? I recently bought a 55 lb box from a glass blowing friend. It is system 96 and the nuggets are just gorgeous and clear. I am going to try a clear casting today but I was wondering if anyone else has tried it yet. It is so affordable at $1 a lb it would be awesome to be able to use it for clear casting.

Thank you
Willi