Getting ready to blow out Color Bar in HOT shop
Hello . I have not posted in awhile and have missed you all so thought I would catch up on what I have been up to. Casting large color bars and then slicing them up to take to the hot shop. Just simply exciting and has allowed me to do things that I could not do before. Working in Bullseye Glass does not stop me from going to the hot shop and Ryan Bavin is truly an inspiration and just knows how to make my ideas and bars into round forms that is a bit more difficult for us all.
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Getting ready to blow out Color Bar in HOT shop
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Getting ready to blow out Color Bar in HOT shop
- Attachments
-
- php8UaO3DAM.jpg (22.68 KiB) Viewed 53501 times
-
- phpMkqarJAM.jpg (61.6 KiB) Viewed 53501 times
Last edited by twin vision glass on Mon Apr 16, 2018 1:19 pm, edited 1 time in total.
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Getting ready to blow out Color Bar in HOT shop
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: Getting ready to blow out Color Bar in HOT shop
impressive work being created.
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Getting ready to blow out Color Bar in HOT shop
Hi Kevin. Hope you are well . I love it back in the hot shop again.
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
Warren Weiss
- Posts: 137
- Joined: Thu Mar 13, 2003 8:06 pm
- Location: Richmond, VA
Re: Getting ready to blow out Color Bar in HOT shop
Beautiful!! A new dimension.
Warren
Warren
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Getting ready to blow out Color Bar in HOT shop
I have really enjoyed getting back into the hot shop and Ryan Bavin just understands so well how the Bullseye Glass Blows out in large chunks and sections and how to maximize the interesting things going on inside. The important part is to remember what will actually be inside when blown out and what is on the outside when all is said and done
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Getting ready to blow out Color Bar in HOT shop
Hot shop fun and happy with Vitrigraph pull on outside
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
Ed Cantarella
- Posts: 155
- Joined: Mon Feb 26, 2018 3:49 pm
- Location: Highland, Michigan, USA
Re: Getting ready to blow out Color Bar in HOT shop
WOW - really gorgeous.
I would really dig manipulating glass like that, after some intense instruction. Too cool.
I would really dig manipulating glass like that, after some intense instruction. Too cool.
HER last words were, "I'm melting, melting . . . " Dissenting opinions generally welcome for comic relief or personal edification. Sometimes both.
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Getting ready to blow out Color Bar in HOT shop
Thank you Ed, I love taking the Bullseye Glass to the hot shop and manipulating it. The large cast glass bars are the best to begin with for me for a more organic look.
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Getting ready to blow out Color Bar in HOT shop
always fun to go get a nice pic
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com
Re: Getting ready to blow out Color Bar in HOT shop
It is so great to see your work posted here again! I’ve missed you! What a wonderful thing for you to once again merge these two glass methodologies. Inspirational. Thank you for posting the pictures of your adventure.
Sharol
Sharol
-
twin vision glass
- Posts: 570
- Joined: Thu Apr 29, 2004 12:55 am
- Location: Invermere,B.C. Canada
- Contact:
Re: Getting ready to blow out Color Bar in HOT shop
Hi Sharol, It is great to share again with everyone. I tooo have missed posting in Warm Glass. My twin and I are having fun pulling out the slices on the torch as well. It is just so fun to take this beautiful material and manipulate it hot.
Give out Free Hugs!
website: http://www.twinvision.fusedglassartists.com
website: http://www.twinvision.fusedglassartists.com