has anyone had any problems with fusing bottles together then Slumping them into a kool form ? Any certain bottles brands to avoid ?
I was thinking of putting a hole bunch of (Rolling Rock) bottles together and slumping them in a wavey mold (bulls eyes)
Any suggeestions or comments on this before I might waste my time ?
Thanks Tyler
Fusing Botltles Together
Moderators: Brad Walker, Tony Smith
-
Tyler Frisby
- Posts: 75
- Joined: Tue Dec 02, 2003 8:27 pm
- Location: Canada
-
Ron Coleman
- Posts: 468
- Joined: Sun Mar 09, 2003 3:20 pm
- Location: Columbus, Ohio USA
-
Tyler Frisby
- Posts: 75
- Joined: Tue Dec 02, 2003 8:27 pm
- Location: Canada
-
Tyler Frisby
- Posts: 75
- Joined: Tue Dec 02, 2003 8:27 pm
- Location: Canada
-
Judy Schnabel
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact:
Tyler,
You can definitely fire together Skyy Blue malt liquor bottles. They are all made by the same manufacturer -- same coe.
As for Rolling Rock -- no problem melting them but I've never put them together.
As for beer bottles, look around the rim on the bottom. There is a code which tells who made the bottle. Try to keep "codes" with "codes." I learned this the hard way with Heineken. Heineken has about five different manufacturers. Keep likes with likes.
Judy
You can definitely fire together Skyy Blue malt liquor bottles. They are all made by the same manufacturer -- same coe.
As for Rolling Rock -- no problem melting them but I've never put them together.
As for beer bottles, look around the rim on the bottom. There is a code which tells who made the bottle. Try to keep "codes" with "codes." I learned this the hard way with Heineken. Heineken has about five different manufacturers. Keep likes with likes.
Judy
-
Tyler Frisby
- Posts: 75
- Joined: Tue Dec 02, 2003 8:27 pm
- Location: Canada