Iso-mag board

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Iso-mag board

Post by Marty »

Anyone have experience with this stuff from Pyrotec (shelves, dams, molds, whatever)?
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Iso-mag board

Post by Brad Walker »

Never heard of it, but it looks interesting. Let me know if you try it out or find out more.
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Iso-mag board

Post by Marty »

Brad- One of my Canadian students uses it instead of VB- it's magnesium salt based, seems to be stronger than VB with less warpage. I asked on Pete's board, we'll see what comes up. I'll also call Jim Wiles (?) and see what he knows.
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Iso-mag board

Post by Brad Walker »

I'm interested in its machine-ability and whether it can take kiln wash. I've been having trouble with vermiculite board leaving a haze on the glass.

Tried calcium silicate boards, they're prone to thermal shock, but perhaps this can work. Let me know what Jim says, if he can get it I can drive down to Charlotte and pick some up to try.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Iso-mag board

Post by Buttercup »

Marty, what's Pete's board, please....another glass site?
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Iso-mag board

Post by Brad Walker »

Buttercup wrote:Marty, what's Pete's board, please....another glass site?
http://talk.craftweb.com/forumdisplay.php?s=&forumid=4
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Iso-mag board

Post by Marty »

Another closely monitored private board, but Pete is more irascible than Brad. It's mostly blowing but there are a few active fusers. No anonymity there.
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Iso-mag board

Post by Brad Walker »

Marty wrote:Pete is more irascible than Brad.
Guess I need to try harder.
Buttercup
Posts: 638
Joined: Mon Jan 28, 2008 5:22 pm
Location: S.E. Queensland Australia

Re: Iso-mag board

Post by Buttercup »

Thanks Brad and Marty. I know of Craftweb, Just haven't heard it referred to as 'Pete's board'. As you say, mostly blowing, so I don't browse it and certainly am not qualified to contribute.
Post Reply