I am looking for a stainless steel double s mold that is 12 inches long by 3 inches wide. Similar to the mold in the picture only longer and a little wider. Does anyone know where I can obtain one or does anyone on the board have a way to make me one?
Thanks in advance,
Peter Brown
mold
Moderators: Brad Walker, Tony Smith
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
Re: mold
It looks like a simple job for a shop that builds custom Hot Rods. They have forming rollers and maybe even a SS source.
"The Glassman"
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: mold
Consider not using stainless. I have these kinds of things made from regular mild steel, as much as 1/4" thick and just cover the steel with thinfire paper before I use the mold. Works perfect, and any spalling is contained by the thinfire.
I use a local metal fabricator. They're fairly easy to deal with and reasonably priced. Three in my area, I just get prices from them all when I have a job to do.
I use a local metal fabricator. They're fairly easy to deal with and reasonably priced. Three in my area, I just get prices from them all when I have a job to do.