Stainless ring mold
Moderators: Brad Walker, Tony Smith
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Stainless ring mold
Made the mistake of using thinfire to line a ring mold for a strip circle..when it came out it is stuck in the mold..the glass is intact so dont think it is stuck to the steel just stuck. any ideas how to salvage this? I'm currently trying to reheat it a bit to see if the steel loosens.
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
-
DonMcClennen
- Posts: 381
- Joined: Sun Mar 09, 2003 9:09 pm
- Location: Ontario
-
Bert Weiss
- Posts: 2339
- Joined: Tue Mar 11, 2003 12:06 am
- Location: Chatham NH
- Contact:
Re: Stainless ring mold
Jim
Stainless steel shrinks more than glass during the cool down, so the ring is holding on to the glass. It is recommended to use a thicker layer of paper which will make up for the expansion differences. So yes, reheat. Try placing the glass raised up on something like a firebrick. Heat at a rate you would reheat, and somewhere above 300, the ring will fall off. Or maybe you can help persuade it to fall off...
Stainless steel shrinks more than glass during the cool down, so the ring is holding on to the glass. It is recommended to use a thicker layer of paper which will make up for the expansion differences. So yes, reheat. Try placing the glass raised up on something like a firebrick. Heat at a rate you would reheat, and somewhere above 300, the ring will fall off. Or maybe you can help persuade it to fall off...
Bert
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
Bert Weiss Art Glass*
http://www.customartglass.com
Furniture Lighting Sculpture Tableware
Architectural Commissions
-
jim burchett
- Posts: 255
- Joined: Sun Jun 29, 2003 4:24 pm
- Location: Lenoir, NC
Re: Stainless ring mold
"No, you cant scare Me, I'm sticking to the UNION. I'm stickin to the UNION till the day I die" Woody Guthrie
Re: Stainless ring mold
Thanks I made a similar error yesterday on a ring mold. Thawing it out to heat it up as I type.
-
Chris Lowry
- Posts: 51
- Joined: Thu Sep 24, 2015 12:35 pm
Re: Stainless ring mold
Any reason you can’t use thicker stainless rings as long as you use fiber paper for a buffer? I have some 1/8” and 1/4” thick rings that were for a different project.
-
Brad Walker
- Site Admin
- Posts: 1542
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: Stainless ring mold
Thicker will work fine.
Or just cut a hole in something like a piece of Ceramaguard and for a lot less money than stainless you'll have something that will work just as well.
Or just cut a hole in something like a piece of Ceramaguard and for a lot less money than stainless you'll have something that will work just as well.
-
Chris Lowry
- Posts: 51
- Joined: Thu Sep 24, 2015 12:35 pm
Re: Stainless ring mold
Thanks Brad, good ideas