Easy Fire enamels

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
Vonon
Posts: 197
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Easy Fire enamels

Post by Vonon »

Is there any difference between Fusemaster high fire opaque enamels and the (new to me) Easy Fire enamels? Also what is the deal with Colors for Earth? Are they re-branded ceramic undercoat glaze? I got distracted from glass work for a couple of years and now have all these new choices to deal with. TIA for any information you could offer.
Vonon
Brad Walker
Site Admin
Posts: 1544
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: Easy Fire enamels

Post by Brad Walker »

Lots of enamels out there, none are the same. You'll have to check the specifications (firing recommendations) and content (lead or non-lead, COE dependent or not) for each enamel to make comparisons.

Since Easy Fire and Fusemaster are marketed by the same people (Fusion Headquarters), I would contact them to ask the specific differences between the two. It's possible that Easy Fire is just the high fire Fusemaster rebranded. Ask them to know for sure.
Vonon
Posts: 197
Joined: Fri Mar 10, 2006 6:32 pm
Location: East Tennessee

Re: Easy Fire enamels

Post by Vonon »

Thank you Brad.
Vonon
Post Reply