fusing glass laminate powder

This is the main board for discussing general techniques, tools, and processes for fusing, slumping, and related kiln-forming activities.

Moderators: Brad Walker, Tony Smith

Post Reply
anne b
Posts: 1
Joined: Wed Nov 19, 2014 11:38 am

fusing glass laminate powder

Post by anne b »

Wondering if glass laminate (Arco) can be used in fusing. A friend gave me many boxes of this substance (old) in many colors. Can't find anything online about it, except that manufactured laminated glass is used as safety glass. Makes me think it might be something plastic. Very fine powder - like talc. Thanks for any info.
Attachments
photo of box
photo of box
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: fusing glass laminate powder

Post by Brad Walker »

In general glass laminate is used to laminate two pieces of glass together (like a front windshield in a car). It's a kind of plastic film between the two and can't be fused in the kiln.