Round piece of glass.....sagging
Moderator: Tony Smith
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Round piece of glass.....sagging
Hello ! I have no idea what will happen when you let sagg a round piece of glass. Is there anywhere a photo of this ?? Thank you, Jan de Jong
-
jim simmons
- Posts: 478
- Joined: Sun Mar 09, 2003 10:37 pm
- Location: Hillsboro Oregon
- Contact:
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Round piece of glass.....sagging
@ Jim Simmons: 26 cm diameter over kilnstands with on the top ceramic thick paper (felt ?). As I did for tealights but then square and not so big. Jan
-
The Hobbyist
- Posts: 311
- Joined: Sun Mar 09, 2003 7:09 pm
- Location: Sun City West (NW Phoenix), AZ
- Contact:
Re: Round piece of glass.....sagging
The circle will sag like the square, by folding in a few places. If centered on the post it will end up with even height edges without the peaks you get with a square drape/sag.
Do a test with a circle of float to see if you get the effect you want.
Jim
Do a test with a circle of float to see if you get the effect you want.
Jim
"With or without religion, good people can behave well and bad people can do evil; but for good people to do evil—that takes religion. " Steven Weinberg
-
Jan de Jong
- Posts: 114
- Joined: Sun Mar 09, 2003 3:31 pm
- Location: The Netherlands
Re: Round piece of glass.....sagging
@ The Hobbyist: Thank you ! I will do a test. Jan de Jong