copper inclusion

Post by Michael Stevens »

I wanted to add this thin copper 2mm thick twisted copper. into a 5inch diameter glass orb. would the metal cause breakage because too thick. leaf or foil wouldn't give the effect I was looking for.

is there a formula for dimension of metal inclusion vs thickness of glass object?
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: copper inclusion

Post by Brad Walker »

2mm is too thick. It will almost certainly crack.

No formula that I'm aware of. It would depend on the particular metal, of course.
Michael Stevens
Posts: 83
Joined: Thu Dec 26, 2019 2:52 pm

Re: copper inclusion

Post by Michael Stevens »

I'm. sorry I meant .2mm
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: copper inclusion

Post by Brad Walker »

Michael Stevens wrote:I'm. sorry I meant .2mm
.2mm should be thin enough. Try a small piece as a test.