2 things for a newbie - safety & skutt kiln message
Moderators: Brad Walker, Tony Smith
-
rowanberry
- Posts: 3
- Joined: Sat Mar 27, 2004 5:35 pm
2 things for a newbie - safety & skutt kiln message
Just got my first kiln & started fusing - I see that Skutt sells vent hoods for their kilns. Do I need to vent the kiln when I am fusing glass, using kiln wash and no fiber paper? What makes the fumes? (I did not smell anything or see anything) Also, I have a Skutt HotStart with a Controller. As it was ramping down, it gave me the message "CPL(?) 5.52 - does anyone know what that means? It's not in the manual, and I will call skutt, but thought I would ask here first since it's the weekend. thanks.
Re: 2 things for a newbie - safety & skutt kiln message
Just got my first kiln & started fusing - I see that Skutt sells vent hoods for their kilns. Do I need to vent the kiln when I am fusing glass, using kiln wash and no fiber paper?
No.
What makes the fumes?
Almost anything other than what you named.
(I did not smell anything or see anything) Also, I have a Skutt HotStart with a Controller. As it was ramping down, it gave me the message "CPL(?) 5.52 - does anyone know what that means? It's not in the manual, and I will call skutt, but thought I would ask here first since it's the weekend. thanks.
That's my license plate!
No.
What makes the fumes?
Almost anything other than what you named.
(I did not smell anything or see anything) Also, I have a Skutt HotStart with a Controller. As it was ramping down, it gave me the message "CPL(?) 5.52 - does anyone know what that means? It's not in the manual, and I will call skutt, but thought I would ask here first since it's the weekend. thanks.
That's my license plate!
My memory is so good, I can't remember the last time I forgot something . . .
-
skin_mechanic
- Posts: 35
- Joined: Fri Mar 26, 2004 10:42 pm
- Location: Birmingham, AL
Howdy there
I'm a fellow Skutt owner, and green as grass
so my 1st answer may be wrong. I don't think you'll have to worry about fumes from the kiln wash, enameling may be another story though. I've been considering buying the EnviroVent to aid in keeping the temps even, and steady. The CPL 5.52 message means the firing process was completed in 5hrs, 52mins. You'll learn alot from these guys, I have, and I've only been here for a day 
-Joseph
-Joseph
-
Jackie Beckman
- Posts: 475
- Joined: Sun Mar 09, 2003 5:01 pm
- Location: Arizona
- Contact:
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
-
rowanberry
- Posts: 3
- Joined: Sat Mar 27, 2004 5:35 pm
Thanks & 1 more question
Thanks for the info, all! If the process was complete in 5.52 hours, then the rest of the time must have been annealing and cool down. Then the question is, once I see the CPL, can I unplug the kiln and go to bed? (I was up every half hour until 4AM and it still read 256 degrees - at which point I did finally unplug it.
-
Jackie Beckman
- Posts: 475
- Joined: Sun Mar 09, 2003 5:01 pm
- Location: Arizona
- Contact:
Re: Thanks & 1 more question
Yes, once it reads CPL it's done so you can just unplug it and go to bed - in fact, that's the BEST thing to do to prevent you from peeking inside before its cooled.rowanberry wrote:Thanks for the info, all! If the process was complete in 5.52 hours, then the rest of the time must have been annealing and cool down. Then the question is, once I see the CPL, can I unplug the kiln and go to bed? (I was up every half hour until 4AM and it still read 256 degrees - at which point I did finally unplug it.
-
Judy Schnabel
- Posts: 195
- Joined: Mon Mar 10, 2003 9:45 pm
- Location: SW FL
- Contact:
-
rosanna gusler
- Posts: 730
- Joined: Mon Mar 10, 2003 2:22 pm
- Location: wanchese north carolina
- Contact:
Re: Thanks & 1 more question
annealing is part of the process. when it says complete it has run through all the segments that you told it to and is cooling naturally. rosannarowanberry wrote:Thanks for the info, all! If the process was complete in 5.52 hours, then the rest of the time must have been annealing and cool down. Then the question is, once I see the CPL, can I unplug the kiln and go to bed? (I was up every half hour until 4AM and it still read 256 degrees - at which point I did finally unplug it.