So, I just bought a used bell kiln, and it arrived damaged. i have decided to rebuild the top with all new fiber board, blanket and elements. Would like to know what elements you guys would recommend, and top only or top and side?

Firing chamber 48x48x18"
240 volt single phase


Want to be able to go to 1850. Not often, but want the capability.

Thanks

Dick
Brad Walker
Site Admin
Posts: 1543
Joined: Fri Mar 07, 2003 9:33 pm
Location: North Carolina, USA
Contact:

Re: bell kiln repair

Post by Brad Walker »

For fiber, top only should work.

For brick, both.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: bell kiln repair

Post by Kevin Midgley »

Kanthal A1