So, I just bought a used bell kiln, and it arrived damaged. i have decided to rebuild the top with all new fiber board, blanket and elements. Would like to know what elements you guys would recommend, and top only or top and side?
Firing chamber 48x48x18"
240 volt single phase
Want to be able to go to 1850. Not often, but want the capability.
Thanks
Dick
bell kiln repair
Moderators: Brad Walker, Tony Smith
-
Brad Walker
- Site Admin
- Posts: 1543
- Joined: Fri Mar 07, 2003 9:33 pm
- Location: North Carolina, USA
- Contact:
Re: bell kiln repair
For fiber, top only should work.
For brick, both.
For brick, both.
-
Kevin Midgley
- Posts: 774
- Joined: Mon Mar 10, 2003 11:36 am
- Location: Tofino, British Columbia, Canada
Re: bell kiln repair
Kanthal A1