Kiln element compatibility with stainless?

This forum is for questions from newcomers to kiln-forming.

Moderator: Tony Smith

Post Reply
Mike Garvey
Posts: 6
Joined: Wed Jan 15, 2020 11:26 am

Kiln element compatibility with stainless?

Post by Mike Garvey »

I am thinking to add a small stainless washer to a kiln element (Kanthal) tail as it passes out of the kiln in order to prevent the tail from cutting into the soft firebrick. Can I use stainless or do I have to go the ceramic route? Thanks....Mike
Marty
Posts: 865
Joined: Mon Mar 10, 2003 3:58 pm
Location: Maine
Contact:

Re: Kiln element compatibility with stainless?

Post by Marty »

Either will work. I used ss fender washers.
Kevin Midgley
Posts: 774
Joined: Mon Mar 10, 2003 11:36 am
Location: Tofino, British Columbia, Canada

Re: Kiln element compatibility with stainless?

Post by Kevin Midgley »

Ceramic tubes are available. Old knob and tube wiring tubes could work as well. Get your wiring inspected before using.